Super Alloy

        Superalloys are alloys that exhibit excellent mechanical strength and creep resistance at high temperatures, good surface stability, and corrosion and oxidation resistance. The corrosion-resistant superalloys are widely used in extreme environments where tremendous heat and corrosion resistance is paramount to the integrity of the end product. Chemical and petrochemical processing, Aero-engines, power plants, and oil and gas industries widely use these superalloys.

      Many of the industrial nickel-based superalloys contain alloying elements, including chromium (Cr), aluminum (Al), titanium (Ti), molybdenum (Mo), tungsten (W), niobium (Nb), tantalum (Ta) and cobalt (Co).
MIDHANI supplies most of the superalloys in the form of sheet, plate and bar forms.
MIDHANI grade Names & designations
1. Nickel alloys – Superni
2. Cobal allloys – Superco
3. Iron alloys – Superfer

Nickel based Alloys

MIDHANI Alloy Name Trade Name UNS No. British Specs American Specs German Specs French Specs
Superni 600 Inconel 600 N06600 BS 3072 AMS 5540 Sheet, Strip and Plate AMS 5665 Bar and Forging ASTM B 168, DTD 328 A NiCr15Fe8 2.4816 AFNOR NC15Fe
Superni 601 Inconel 601 N06601 AMS 5715 Bar and Forgings AMS 5870 Sheet, Strip and Plate 2.4851
ASTM B166
Superni 617 Inconel 617 N06617 AMS 5887 Bar and Forgings AMS 5888 Plate NiCr23Co12Mo WS 2.4663
Superni 625 Inconel 625 N06625 BS 3072 AMS 5666 Bar, Forgings AMS 5869 Sheet, Strip and Plate NiCr22Mo9Nb 2.4856 AFNOR NC22DNb
Superni 690 Inconel 690 N06690 ASTM B 163 2.4642
Superni 706 Inconel 706 N09706 AMS 5701 Bar and Forgings
Superni 718 Inconel 718 N07718 AMS 5662 Bar and Forgings AMS 5596 Sheet, Strip and Plate NiCr19Fe19Nb5Mo3 2.4668
Superni 750 Inconel X750 N07750 AMS 5542 Sheet, Strip and Plate AMS 5747 Bar and Forgings 2.4669
Superni 740H
Superni C276 Inconel C276 Hastelloy C276 N10276 ASTM B575 NiMo16 Cr15W 2.4819
Superni 75 Nimonic 75 Haynes 75 N06075 BS HR5 BS HR203 2.4630 2.4951 AFNOR NC 20T
Superni 76 Hastelloy X N 06002 AMS 5754 AMS 5536 NiCr22Fe18Mo 2.4665
Superni 80A Nimonic 80A N07080 BS HR1 Alloy 80A Bar ASTM B637 NiCr20TiAl 2.4952 AFNOR NC 20TA
Superni 90 Nimonic 90 N07090 BS HR2 Alloy 90 bar BS HR202 Alloy 90 sheet AMS 5829 Welding Wire 2.4632
Superni 263 Nimonic 263 Haynes 263 N07263 BS HR10 BS HR206 BS HR404 AMS 5872 Sheet and Plate AMS 5886 Bar and Forgings NiCo20Cr20Mo6Ti2Al 2.4650
Superni 105 Nimonic 105 BS HR3 2.4634 AFNOR NCKD 20ATv
Superni 115 Nimonic 115 BS HR4 2.4636 AFNOR NCK 15ATD
Superni 100 IN 100 N13100 AMS 5397
Supercast 713C Inconel 713C
Supercast 247A CM 247 MAR M 247

Cobalt based Alloys

MIDHANI Alloy Name Trade Name UNS No. British Specs American Specs German Specs French Specs
Superco 605 Haynes 25 Udimet L605 UNS R30605 AMS 5537 Sheet AMS 5759 Bar & Rod
Superco 35 MP35N UNS R30035 AMS 5844
Superco 783 Inconel 783 R30783 AMS 5940

Iron based Alloys

MIDHANI Alloy Name Trade Name UNS No. British Specs American Specs German Specs French Specs
Superfer 800/800H Incoloy 800 Incoloy 800H N08800 N08810 BS 3072 AMS 5766 Bar and Forgings AMS 5871 Sheet, Strip and Plate ASTM B408 X8 NiCrAlTi 32-21 1.4876 1.4958 1.4959
Superfer 825 Incoloy 825 UNS N08825 BS 3072 ASTM B425 ASTM B424 NiCr 21 Mo 2.4858
Superfer A286 Incoloy A-286 S66286 ASTM A 453 AMS 5525 AMS 5731 X5 NiCrTi 26-15  1.4980